Fraunhofer institute

Fraunhofer institute

The most important results achieved in this test were:

Average TriboCeramic material growth in cylinder walls(restoration) 5 microns
Roughness of the Cylinder Walls after treatment 1,2 Ra (6,6 Ra) = 1/5,5
Average Cylinder Compression increase in TUV test 12 %
Engine Function without engine oil (smooth, normal temp) at least 1 h

 

     Fraunhofer Institute Test